Formula | ZrO2:Y (9.5 mol% Y2O3) |
Growth method | Skull melting |
Max. sizes, (mm) | Ø50.8 |
Transmission range, (µm) (Thickness 15 mm) |
0.43 – 5.0 |
Structure | cubic |
Density (g/cm3) | 5.92 |
Melting point (°C) | 2780 |
Hardness (Mohs) | 8.7 |
Thermal expansion coefficient (10-6/K) | 9.2 |
Thermal conductivity (W m-1 K-1) | 1.8 |
Thermal optical coefficient (10-6/K) | |
Solubility in water (g/100 cm3) | undeclared |
Solubility in acids | undeclared |
Solubility in organic solvents | undeclared |
Wavelength (µm) Refractive index |
4.0 2.24 |
Absorption coefficient (cm-1) |